LOCTITE SF7701

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SF7701

Main features

  • Low-Energy Plastic Priming
  • Fast 30-Second Drying
  • UV-Visible Primer Inspection

Product Description

LOCTITE SF 7701 Primer is a clear, one-part n-heptane primer for preparing polyolefin and other low-energy surfaces for bonding with LOCTITE cyanoacrylate adhesives. The very-low-viscosity liquid contains 0.08% to 0.12% active ingredient, dries in 30 seconds or less at 20 deg C, and remains active on the part for up to 8 hours. It is intended for difficult-to-bond materials including polyethylene, polypropylene, PTFE, and thermoplastic rubber. The primer also accelerates cyanoacrylate fixture, while maximum bond strength develops after 24 hours at 22 deg C.

Key features

  • Low-energy surface priming: Prepares polyethylene, polypropylene, PTFE, and thermoplastic rubber for cyanoacrylate bonding.
  • Fast 30-second drying: Dries in 30 seconds or less at 20 deg C before adhesive application.
  • UV-visible primer inspection: Primer presence can be checked with a 365 nm UV inspection lamp.

Applications

Applications include priming low-energy plastics for LOCTITE cyanoacrylate bonding.

Product Family

LOCTITE SF7701

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Clear colorless liquid
Chemistry Type Chemistry Type
Aliphatic amine
Solvent Solvent
n-heptane
Specific Gravity Specific Gravity
0.68
Physical Properties
Drying Time Drying Time
<30 seconds
Viscosity Viscosity
1.25 mPa.s

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Clear colorless liquid As supplied
Active ingredient concentration 0.08 to 0.12 % Aliphatic amine
Fluorescence Positive Under UV light
Specific gravity 0.68 25 deg C
Viscosity 1.25 mPa s (cP) 20 deg C

Leading Brands Trust in Our Products and Services