LOCTITE LB8504

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE LB8504

Main features

  • Non-Metallic Conductive Anti-Seize
  • 482 deg C Operating Range
  • 0.13 Steel Fastener Torque Coefficient

Product Description

LOCTITE LB 8504 is a one-component, non-metallic graphite and petrolatum anti-seize paste for threaded and fitted metal joints. The dark gray paste is applied full strength to machine threads, tapered pipe threads, press-fit joints and slip-fit joints. It has a typical penetration of 310 to 360 in 0.1 mm units under ISO 2137 and a specific gravity of 1.18 at 25 deg C. The formulation is electrically conductive in metal-to-metal joints and supports an operating range from -29 to 482 deg C. A torque coefficient of 0.13 is reported on the specified steel bolt-and-nut configuration.

Key features

  • Non-metallic graphite paste: Synthetic graphite and petrolatum provide anti-seize lubrication without metallic solids.
  • High-temperature joint service: The applied paste supports use from -29 to 482 deg C.
  • Controlled torque response: A torque coefficient of 0.13 is reported on the specified steel fastener configuration.

Applications

Applications include machine threads, tapered pipe threads, press-fit joints, slip-fit joints and anti-seize lubrication of metal assemblies.

Technical Specifications

General Properties
Appearance Appearance
Dark gray past
Chemistry Type Chemistry Type
Graphite-Based
Component System Component System
One component
Specific Gravity Specific Gravity
1.18

Additional Information

Technical properties

As-supplied properties

Typical as-supplied product values.

Property Value Unit Method / condition
AppearanceDark gray pasteAs supplied
ComponentsOne componentNo mixing required
Specific gravity1.18At 25 deg C
Penetration310 to 3600.1 mmISO 2137
Weight per gallon9.5 to 10.4lb/galAs supplied
Optimal storage8 to 21deg CUnopened container in a dry location
Technical properties

After-application / in-service properties

After-application and in-service behavior under the stated joint configuration.

Property Value Unit Method / condition
Operating temperature range-29 to 482deg CApplied anti-seize paste
Torque coefficient0.1312.7 mm grade 8 steel bolts with grade 5 nuts
Unlubricated torque coefficient0.27Same bolt-and-nut configuration, solvent cleaned
Electrical behaviorConductiveMetal-to-metal joints