LOCTITE LB8009

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8009

Main features

  • Steel Compatibility Paste Material
  • Improved Clamp Load Consistency
  • Non-Curing Assembly Formulation

Product Description

LOCTITE® LB 8009® Heavy Duty Anti-Seize is a premium graphite and calcium fluoride based anti-seize lubricant formulated to protect threaded assemblies and metal components exposed to extreme temperatures and harsh industrial environments. The metal-free formulation contains no lead, copper, sulfur, or related compounds, making it compatible with stainless steel and nickel alloys. It provides long-term lubrication, prevents galling and seizure, and facilitates disassembly of components operating from -29°C to +1315°C.

Key Features & Benefits

  • Graphite and calcium fluoride anti-seize formulation.
  • Free from lead, copper, sulfur and free metals.
  • Compatible with stainless steel and nickel alloys.
  • Protects against galling, seizing and corrosion.
  • Provides improved clamp load consistency.
  • Suitable for extremely high temperature applications.
  • Non-curing lubricant paste.

Recommended Applications

  • Bolts, screws, studs and nuts.
  • Pipe joints, plugs and bushings.
  • Extrusion and forming dies.
  • Heat exchangers and shear blades.
  • Metal bending and mechanical packings.
  • Chemical plants, refineries, power plants and steel mills.
  • Marine, aerospace and industrial maintenance applications.
Product Family

LOCTITE LB8009

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Grey paste
Specific Gravity Specific Gravity
1.15

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Anti-Seize Lubricant — Graphite / calcium fluoride formulation
Appearance Grey Paste — Non-curing
Specific Gravity 1.15 — 25°C
Penetration 270 - 370 0.1 mm ISO 2137
Weight per Gallon 9.6 - 10.6 lb/gal Typical
Metal Content None — Lead, copper and sulfur free
Compatibility Stainless Steel & Nickel Alloys — Suitable for corrosion-sensitive assemblies
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -29 to +1315 °C Continuous service range
Torque Coefficient (K Factor) 0.16 — Lubricated 12.7 mm grade 8 steel bolt
Torque Coefficient (K Factor) 0.27 — Unlubricated solvent-cleaned bolt
Clamp Load Efficiency Improved — Provides higher clamp load at equivalent torque
Clamp Load Uniformity Enhanced — More consistent bolt preload distribution
Corrosion Protection Excellent — Protects threaded assemblies from seizure
Galling Resistance Excellent — For stainless steel and alloy assemblies
Disassembly Protection Prevents Seizing — Facilitates future maintenance

Leading Brands Trust in Our Products and Services