LOCTITE ES6010

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE ES6010

Main features

  • Low-Viscosity Electronics Potting
  • 80-to-100-Minute Working Time
  • Room-Temperature or Heat Cure

Product Description

LOCTITE STYCAST ES 6005 / ES 6010 is a two-component, low-viscosity epoxy potting and encapsulating system. Black ES 6005 resin and clear ES 6010 hardener mix at 3.1:1 by volume or 100:20 by weight to produce a black compound with a typical mixed viscosity of 1,700 mPa s at 25 deg C. The system has an 80 to 100 minute working time for a 200 g mass at 25 deg C and cures at room temperature. The cured material is resilient, reaches Shore D 80 hardness and has electrical insulation properties for general-purpose electronics potting.

Key features

  • Low mixed viscosity: A typical mixed viscosity of 1,700 mPa s at 25 deg C supports cavity filling.
  • Extended working time: The mixed 200 g mass provides 80 to 100 minutes of working time at 25 deg C.
  • Room-temperature cure: The system cures in 24 hours at 25 deg C, with a 2 hour cure at 66 deg C.

Applications

Applications include general-purpose potting and encapsulation of electronic assemblies using the complete ES 6005 / ES 6010 system.

Technical Specifications

Physical Properties
Viscosity Viscosity
1,700 mPa.s
Viscosity (Part A) Viscosity (Part A)
11,000 mPa.s
Viscosity (Part B) Viscosity (Part B)
180 mPa.s
General Properties
Appearance Appearance
Black
Chemistry Type Chemistry Type
Epoxy
Mix Ratio Mix Ratio
5:1
Specific Gravity Specific Gravity
1.48
Work life @25°C Work life @25°C
80 to 100 minutes hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
27 °C
Electrical Properties
Dielectric Strength Dielectric Strength
14.37 kV/mm
Volume Resistivity Volume Resistivity
6.03×10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Component and mixed-system values before cure.

Property Value Unit Method / condition
Resin appearanceBlackLOCTITE STYCAST ES 6005, Component A
Hardener appearanceClearLOCTITE STYCAST ES 6010, Component B
Mix ratio by volume3.1:1Part A to Part B
Mix ratio by weight100:20Component A to Component B
Resin viscosity11,000mPa sSpindle 5, 20 rpm, 25 deg C
Hardener viscosity180mPa sSpindle 1, 20 rpm, 25 deg C
Mixed viscosity1,700mPa sSpindle 4, 2 rpm, 25 deg C
Working time80 to 100minutes200 g mass at 25 deg C
Technical properties

Final-state properties

Typical cured-system values; recommended cure is 24 hours at 25 deg C or 2 hours at 66 deg C.

Property Value Unit Method / condition
Shore hardness80Shore DTypical cured system
Glass transition temperature27deg CTypical cured system
Coefficient of thermal expansion below Tg44 x 10^-6mm/mm deg CTypical cured system
Coefficient of thermal expansion above Tg130 x 10^-6mm/mm deg CTypical cured system
Dielectric strength365V/milTypical cured system
Dielectric constant / dissipation factor4.37 / 0.008At 1 kHz and 25 deg C
Volume resistivity6.03 x 10^14ohm-cmTypical cured system
Insulation resistance1.14 x 10^13ohmsTypical cured system