LOCTITE EA 9658.100

Main features

  • Non-Woven Glass Film Support
  • 177 deg C High-Temperature Cure
  • Extended 15-Day Assembly Window

Product Description

LOCTITE EA 9658.100 PSF NWG AERO is the 0.100 lb/sf non-woven glass-supported configuration of a high-temperature epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The film cures for 1 hour at 177 deg C and provides at least 15 days of open assembly time at 25 deg C or 10 days at 32 deg C. Its non-woven glass carrier supports the specified film construction, while controlled flow helps limit hole blockage and excess flash. Refrigerated storage at -18 deg C or below provides a 9-month warranty life.

Key features

  • Non-woven glass support: The 0.100 lb/sf NWG configuration uses a non-woven glass fabric carrier.
  • High-temperature cure: The film cures for 1 hour at 177 deg C under maintained pressure.
  • Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.

Applications

Applications include high-temperature nacelle metal, composite and honeycomb bonding where the 0.100 lb/sf NWG configuration is specified.

Product Family

LOCTITE EA 9658.100

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied properties

Configuration-specific and common EA 9658 handling values.

Property Value Unit Method / condition
ConfigurationEA 9658 .100 PSF NWGSpecific product variant
ConstructionNon-woven glass supportedNWG film
Standard package36 in x 150 ft450 sf roll
Open assembly timeAt least 15daysAt 25 deg C
Open assembly timeAt least 10daysAt 32 deg C
Storage temperature-18 or belowdeg CSealed container
Warranty life9monthsAt -18 deg C or below, from shipment
Cure schedule1 hour at 177 deg CHeat-up rate 2.2 to 4 deg C/minute