LOCTITE EA 9394.2

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9394.2

Main features

  • Thixotropic Gap-Filling Control
  • Fast 4-Hour Set
  • 24-Hour Room-Temperature Cure

Product Description

LOCTITE EA 9394.2 AERO is a two-part, thixotropic structural epoxy paste adhesive for room-temperature aerospace bonding, potting, filling and liquid-shim applications. Its non-sag paste consistency provides gap-filling control, and the adhesive reaches set in 4 hours with complete cure in 24 hours. Packaging ranges from dual cartridges with static mixers to bulk pint, quart and 5-gallon systems. Applications include structural bonding, localized potting and filling, and liquid-shim installation where controlled paste placement is required.

Key features

  • Thixotropic gap filling: The non-sag structural paste is suited to filling gaps and liquid-shim geometries.
  • Fast room-temperature set: Set develops in 4 hours at room temperature.
  • Complete 24-hour cure: The two-part adhesive reaches complete cure in 24 hours at room temperature.

Applications

Applications include structural bonding, potting, filling and liquid-shim installation in aerospace assemblies.

Product Family

LOCTITE EA 9394.2

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied properties

Supplied-system and storage information.

Property Value Unit Method / condition
System formatTwo-part structural pastePart A and Part B
Application behaviorThixotropicGap filling and non-sag placement
Shelf life - Part A1yearStored below 4 deg C or below 28 deg C
Shelf life - Part B1yearStored below 4 deg C or below 28 deg C
PackagingDual cartridge, pint, quart or 5-gallon systemStatic-mixer and bulk configurations