LOCTITE EA 11C

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

LOCTITE EA 11C

Main features

  • Machinable, Low-Outgassing Cured Material
  • Bonds Metals, Most Plastics and Wood
  • Room-Temperature or Heat Cure

Product Description

LOCTITE EA 11C is a black, two-part epoxy adhesive and sealant for general-purpose bonding, sealing, and repair of metals, most plastics, and wood. The resin and hardener mix at 100:38 by weight or 2.5:1 by volume and provide at least 20 minutes of pot life at 25 °C. The system cures at room temperature or with heat, reaches handling strength in approximately 3 to 4 hours at 25 °C, and develops full cure after 72 hours at 25 °C. Once cured, the material can be machined and sanded and has documented high-service-temperature and low-outgassing characteristics.

Key features

  • Multi-material bonding and repair for metals, most plastics, and wood.
  • Room-temperature or heat cure with at least 20 minutes of pot life at 25 °C.
  • Machinable, low-outgassing cured material with documented high-service-temperature capability.

Applications / Suitable for

  • General-purpose bonding, sealing, and repair of metals, most plastics, and wood.

Technical Specifications

General Properties
Appearance Appearance
Black / Green
Component System Component System
Two (Resin / Hardener)
Mix Ratio Mix Ratio
100 : 38 by weight
Pot Life Pot Life
≥20 minutes
Specific Gravity Specific Gravity
1.6 / 1.67
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
114 °C
Thermal Conductivity Thermal Conductivity
0.75 W/m.K
Electrical Properties
Dielectric Strength Dielectric Strength
18.5 kV/mm
Volume Resistivity Volume Resistivity
5.0×10¹⁴ Ohms⋅cm
Other Properties
Storage Temperature Storage Temperature
8-21 °C