LOCTITE CAT 15 LV

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE CAT 15-LV

Main features

  • Low-Viscosity Epoxy Hardener
  • 120-Minute Working Time
  • Rigid/Semi-Rigid/Flexible Epoxy Systems

Product Description

LOCTITE® CAT 15LV™ is a low-viscosity epoxy hardener specifically formulated for use with LOCTITE ABLESTIK® 45LV epoxy resin systems. The hardener enables the formulation of rigid, semi-rigid or flexible adhesive systems depending on the resin-to-hardener ratio used. It provides room-temperature or accelerated heat curing, excellent adhesion to metals, glass and plastics, and is particularly effective for bonding dissimilar substrates. The system offers adjustable flexibility, good electrical insulation properties and dependable mechanical performance across a wide operating temperature range.

Key Features & Benefits

  • Low-viscosity epoxy hardener for ABLESTIK 45LV systems.
  • Adjustable rigid, semi-rigid or flexible cure profiles.
  • Room-temperature or heat-cure capability.
  • Good adhesion to metals, plastics and glass.
  • Suitable for bonding dissimilar materials.
  • Good electrical insulating properties.
  • Long working time for assembly operations.

Recommended Applications

  • General-purpose industrial bonding.
  • Metal-to-plastic assemblies.
  • Glass-to-metal bonding.
  • Electrical and electronic assembly.
  • Applications requiring tunable flexibility.
Product Family

LOCTITE CAT 15 LV

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Product Type Epoxy Hardener — LOCTITE CAT 15LV
Appearance Black Liquid — Component B
Viscosity 11,000 mPa·s (cP) Uncured hardener
Specific Gravity 0.97 — 25°C
Recommended Mix Ratio (Rigid) 100 : 25 Resin : Hardener By weight
Recommended Mix Ratio (Semi-Rigid) 100 : 50 Resin : Hardener By weight
Recommended Mix Ratio (Flexible) 100 : 100 Resin : Hardener By weight
Shelf Life 12 months 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Working Time (Rigid) 120 minutes 100 g mass at 25°C
Working Time (Semi-Rigid) 90 minutes 100 g mass at 25°C
Working Time (Flexible) 90 minutes 100 g mass at 25°C
Recommended Cure Schedule 16 - 24 hours 25°C room temperature cure
Accelerated Cure 30 - 60 minutes 90°C
Operating Temperature (Rigid) -40 to +90 °C Typical service range
Glass Transition Temperature (Rigid) 68 °C ISO 11357-2
Thermal Conductivity 0.4 W/m·K Rigid, Semi-rigid and Flexible systems
Dielectric Breakdown Strength 16 kV/mm IEC 60243-1
Volume Resistivity >1 × 10¹⁵ Ω·cm IEC 60093
Lap Shear Strength (Rigid, Aluminum) 17 N/mm² ISO 4587, tested at 25°C

Leading Brands Trust in Our Products and Services