LOCTITE CAT 15

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE CAT 15

Main features

  • Liquid Polyamide Epoxy Hardener
  • Two-Hour Pot Life
  • 80 deg C Accelerated Cure

Product Description

LOCTITE® CAT 15™ is a liquid polyamide-based epoxy hardener designed for use with compatible LOCTITE STYCAST® epoxy encapsulation, casting and potting systems. The hardener provides room-temperature curing capability, adjustable flexibility, long working life and excellent chemical resistance. Its low-toxicity profile and wide mixing ratio tolerance make it suitable for electrical insulation, electronic encapsulation and industrial composite applications where flexible, durable epoxy systems are required.

Key Features & Benefits

  • Polyamide epoxy hardener for epoxy resin systems.
  • Room-temperature or accelerated heat cure capability.
  • Provides flexible and durable cured systems.
  • Long working and pot life.
  • Good chemical and environmental resistance.
  • Suitable for potting, encapsulation and casting applications.
  • Compatible with electronic and electrical insulation systems.

Recommended Applications

  • Electronic component encapsulation.
  • Electrical potting and insulation systems.
  • Epoxy casting and composite fabrication.
  • Industrial maintenance and repair compounds.
  • Applications requiring flexible epoxy performance.
Product Family

LOCTITE CAT 15

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Product Type Epoxy Hardener — LOCTITE CAT 15 CLR
Technology Polyamide Cure System — Epoxy curing agent
Appearance Amber Liquid — As supplied
Odor Odorless — Ambient conditions
Density 0.98 g/cm³ 20°C
pH 10 — 100% product at 20°C
Flash Point >150 °C Closed cup
Initial Boiling Point >200 °C Typical value
VOC Content <3 % 2010/75/EC
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Pot Life (Reference Data) 2 hours 100 g mass at 25°C
Recommended Room Temperature Cure 16 - 24 hours Typical epoxy system cure
Accelerated Heat Cure 2 hours 80°C
Continuous Service Temperature 90 °C Typical cured system
Intermittent Service Temperature 120 °C Typical cured system
Skin Sensitization Classification Category 1 — H317
Skin Corrosion Classification Category 1B — H314
Environmental Classification Aquatic Chronic 2 — H411
Bioaccumulation Concern vPvB Substance Present — Contains hydrogenated terphenyl