LOCTITE AA 3341

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE AA 3341

Main features

  • Low-Viscosity Thermoplastic Bonding
  • Fast UV/Visible-Light Cure
  • Flexible 220% Elongation

Product Description

LOCTITE AA 3341 is a one-part, low-viscosity acrylated urethane adhesive for UV or visible-light bonding and potting. The transparent, light-yellow liquid has a typical viscosity of 525 mPa s at 25 deg C and fluoresces under UV light for inspection. It is intended primarily for heavily plasticized PVC and also adheres to polycarbonate and ABS. Under the stated cure condition, the cured material reaches 220% elongation at break, giving the bondline a flexible profile where compliance is important. Applications include disposable medical-device assembly and thermoplastic component bonding.

Key features

  • Low-viscosity dispensing: A typical viscosity of 525 mPa s at 25 deg C supports controlled application.
  • Flexible cured profile: The cured material reaches 220% elongation at break under the stated cure condition.
  • UV fluorescence: Positive fluorescence supports visual confirmation of adhesive presence.

Applications

Applications include bonding heavily plasticized PVC, polycarbonate and ABS, potting, and disposable medical-device assembly.

Product Family

LOCTITE AA 3341

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values unless otherwise stated.

Property Value Unit Method / condition
AppearanceTransparent light yellow liquidUncured
Specific gravity1.09At 25 deg C
Viscosity525mPa sBrookfield RVT, spindle 1, 10 rpm, 25 deg C
UV fluorescencePositiveInspection under UV light
Optimal storage range8 to 21deg CUnopened container in a dry location
Technical properties

Final-state properties

Typical cured-material values after 30 mW/cm^2 at 400 nm for 30 seconds using an indium-doped metal-halide source, unless otherwise stated.

Property Value Unit Method / condition
Shore hardness27Durometer DISO 868
Elongation at break220%ISO 527-3
Tensile modulus25N/mm^2ISO 527-3
Tensile strength at break15N/mm^2ISO 527-2
UV depth of cure4.0mmStated cured-material condition
Block shear strength6.2N/mm^2ISO 13445, polycarbonate to PVC
Dielectric breakdown strength31.5kV/mmCured material