LOCTITE 8060

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 8060 LOCTITE 8060

Main features

  • High-Temperature Anti-Seize Protection
  • Controlled Stick Application
  • Measured Assembly Torque Behavior

Product Description

LOCTITE LB 8060 is a silver, non-curing anti-seize lubricant supplied as an application stick for threaded and closely fitted metal parts. The naphthenic-oil formulation supports controlled placement on fine threads, snug slip fits, boiler and oven components, jet-engine hardware, and industrial turbines within the product's service limits. Typical use extends to 870 deg C, and the torque coefficient is 0.18 on 3/8 x 16 steel nuts and bolts. It is not a high-speed load-carrying lubricant and must not be used on ball or roller bearings or parts where lubrication is critical.

Key features

  • High-temperature anti-seize protection: Typical use reaches up to 870 deg C for threaded and closely fitted metal assemblies.
  • Controlled stick application: The solid format supports direct placement without dispensing a loose paste.
  • Measured assembly torque behavior: A torque coefficient of 0.18 is reported on 3/8 x 16 steel nuts and bolts.

Applications / Suitable for

  • Anti-seize protection for fine threads
  • Snug slip fits and closely mated metal parts
  • High-temperature boiler, oven, turbine, and jet-engine hardware within listed limits

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Naphthenic oil
Color Color
Silver color/ Stick
Component System Component System
One component
Specific Gravity Specific Gravity
1.1
Chemical Properties
Copper Corrosion Copper Corrosion
Slight tarnish, 1a

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceSilver-As supplied
Product formStick-As supplied
Base fluidNaphthenic oil-Formulation description
Cure behaviorNon-curing-As supplied and in service
Specific gravity1.1-25 deg C
Penetration20 to 800.1 mmISO 2137
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Typical use temperatureUp to 870deg CTypical use guidance
Torque coefficient0.18-3/8 x 16 steel nuts and bolts
Copper corrosion rating1a, slight tarnish-ISO 2160
Dimensional stabilityPass-77 deg C

Leading Brands Trust in Our Products and Services