LOCTITE 635

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 635 LOCTITE 635 LOCTITE 635 LOCTITE 635

Main features

  • High-Strength Cylindrical Retention
  • Medium-Viscosity Application Control
  • Anaerobic One-Part Metal Cure

Product Description

LOCTITE 635 is a green, medium-viscosity one-component anaerobic retaining compound for high-strength bonding of cylindrical metal parts. It fills the clearance between close-fitting components and cures after air is excluded, locking rotors on shafts, bushings and sleeves, and press-fit assemblies. A 1,500 to 2,500 mPa s viscosity supports controlled application before assembly. The cured material develops measured compressive-shear strength on steel pins and collars, with strength increasing under the specified heat-cure schedules. This high-strength grade is intended for joints where permanent retention is preferred over routine disassembly.

Key features

  • High-strength cylindrical retention: Measured steel pin-and-collar shear values support permanent retaining applications.
  • Medium-viscosity placement control: A 1,500 to 2,500 mPa s viscosity supports controlled coverage of cylindrical fits.
  • Anaerobic one-part cure: The compound cures in confined metal joints without mixing.

Applications / Suitable for

  • Retaining rotors on shafts
  • Locking bushings and sleeves
  • Augmenting press-fit cylindrical assemblies

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Dimethacrylate ester
Color Color
Green opaque liquid
Component System Component System
One component
Specific Gravity Specific Gravity
1.1
Thermal Properties
Linear thermal expansion Linear thermal expansion
80×10^-6 K -1
Specific Heat Capacity Specific Heat Capacity
0.3 J/(g⋅°C)
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity Viscosity
1,500 to 2,500 mPa.s
Mechanical Properties
Elongation Elongation
<2 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceGreen opaque liquid-As supplied
Chemical typeDimethacrylate ester-One-component material
Specific gravity1.1-25 deg C
Viscosity1,500 to 2,500mPa sBrookfield RVT, spindle 3, 20 rpm, 25 deg C
Cure mechanismAnaerobic-Confined between close-fitting metal surfaces
Strength classHigh strength-Retaining-compound positioning
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Elongation at break<2%Cured material
Compressive shear strength>=13.8N/mm^2Steel pins and collars; 30 min at 22 deg C with Activator 7471 on one side
Compressive shear strength>=20N/mm^2Steel pins and collars; cured 24 h at 22 deg C
Compressive shear strength>=31N/mm^2Steel pins and collars; cured 1 h at 93 deg C, tested at 22 deg C
Compressive shear strength>=9.6N/mm^2Steel pins and collars; 1 h at 93 deg C plus 1 h at 149 deg C, tested at 149 deg C