LOCTITE 571

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 571

Main features

  • Medium-Viscosity Tapered-Thread Sealing
  • Anaerobic One-Part Retention
  • Fluid-Exposure Strength Retention

Product Description

LOCTITE 571 is a brown, medium-viscosity one-component anaerobic thread sealant for locking and sealing metal tapered threads and fittings. The methacrylate liquid cures in confined metal joints after air is excluded, with activator-supported cure available where the application process requires it. Its viscosity range supports controlled coverage without the very free flow of lower-viscosity grades. The cured sealant has medium-strength retention and measured prevailing-torque performance. Properly tightened fittings can seal immediately to moderate pressure, while a 24-hour cure supports maximum pressure and solvent resistance.

Key features

  • Controlled tapered-thread coverage: A 1,000 to 10,000 mPa s viscosity supports application to metal tapered threads and fittings.
  • Anaerobic one-part cure: The material cures in confined metal joints without component mixing.
  • Fluid-exposure strength retention: Tested joints retained initial strength after specified 720-hour fluid exposures at 87 deg C.

Applications / Suitable for

  • Locking metal tapered threads
  • Sealing metal pipe fittings
  • Assemblies requiring medium-strength service retention

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Methacrylate ester
Color Color
Brown liquid
Component System Component System
One component
Specific Gravity Specific Gravity
1.1
Thermal Properties
Linear thermal expansion Linear thermal expansion
0.1×10^-6 K -1
Specific Heat Capacity Specific Heat Capacity
0.3 J/(g⋅°C)
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity Viscosity
1,000 to 10,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceBrown liquid-As supplied
Chemical typeMethacrylate ester-One-component material
Specific gravity1.1-25 deg C
Viscosity1,000 to 10,000mPa sBrookfield RVF, spindle 3, 20 rpm, 25 deg C
Cure mechanismAnaerobic-Confined between close-fitting metal surfaces
Secondary cure supportActivator-When specified for the application
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Prevailing torque after 6 h0.6 to 2.8N m3/8 x 24 grade 2 steel fasteners, 22 deg C
Prevailing torque after 24 h1.1 to 2.8N m3/8 x 24 grade 2 steel fasteners, 22 deg C
Strength retention in motor oil100% of initial720 h at 87 deg C
Strength retention in unleaded gasoline100% of initial720 h at 87 deg C
Strength retention in phosphate ester100% of initial720 h at 87 deg C
Strength retention in acetone100% of initial720 h at 87 deg C
Strength retention in distilled water100% of initial720 h at 87 deg C