LOCTITE 420

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 420

Main features

  • Very-Low-Viscosity Capillary Bonding
  • Fast Close-Fitting Assembly
  • Broad Metal-Plastic-Rubber Bonding

Product Description

LOCTITE 420 is a one-component, very-low-viscosity ethyl cyanoacrylate instant adhesive for general-purpose bonding of plastics, rubbers, and metals. The transparent, colorless-to-straw liquid requires no mixing and cures with atmospheric moisture. At 22 deg C and 50% relative humidity, fixture times range from under 5 seconds on neoprene and nitrile rubber to 5 to 15 seconds on aluminum and 10 to 30 seconds on degreased mild steel. After 24 hours at 22 deg C, grit-blasted steel lap shear strength is 15 to 26 N/mm^2. The material is intended for thin, close-fitting bond gaps.

Key features

  • Very-Low-Viscosity Flow: A 1 to 5 mPa s viscosity supports capillary flow into thin, close-fitting joints.
  • Fast Close-Fitting Assembly: Neoprene and nitrile fixture in under 5 seconds under the listed ambient condition.
  • Broad Substrate Bonding: The adhesive bonds plastics, rubbers, and metals with substrate-specific strength data.

Applications / Suitable for

  • General-purpose plastic bonding
  • Rubber and elastomer bonding
  • Thin, close-fitting metal joints

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Ethyl cyanoacrylate
Color Color
Transparent, colorless to straw colored liquid
Component System Component System
One component
Specific Gravity Specific Gravity
1.05
Thermal Properties
Linear thermal expansion Linear thermal expansion
100×10^-6 K -1
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity Viscosity
1 to 5 mPa.s
Electrical Properties
Dielectric Strength Dielectric Strength
25 kV/mm
Volume Resistivity Volume Resistivity
2×10^15 Ohms⋅cm
Curing Conditions
Fixture Time Fixture Time
10 to 30 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw-Uncured
Specific gravity1.05-25 deg C
Viscosity1 to 4mPa sCone and plate, shear rate 3,000 s^-1, 25 deg C
Viscosity1 to 5mPa sBrookfield LVF, spindle 1, 6 rpm, 25 deg C
Vapor pressure<1hPaAs supplied
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion100 x 10^-6K^-1ISO 11359-2; cured 24 hours at 22 deg C
Thermal conductivity0.1W/(m K)ISO 8302; same cure
Softening point165deg CDIN EN 1427; cured material
Dielectric breakdown strength25kV/mmIEC 60243-1; cured material
Lap shear strength15 to 26N/mm^2Grit-blasted steel; cured 24 hours at 22 deg C
Lap shear strength12 to 19N/mm^2Grit-blasted aluminum; cured 24 hours at 22 deg C
Tensile strength12 to 25N/mm^2ISO 6922; steel; cured 24 hours at 22 deg C