LOCTITE 416

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 416

Main features

  • High-Viscosity One-Part Cyanoacrylate
  • Documented MIL-A-46050C/A-A-3097 Qualification
  • Multi-Material Plastic/Rubber/Metal Bonding

Product Description

LOCTITE® 416™ is a one-component, high-viscosity ethyl cyanoacrylate instant adhesive formulated for general-purpose bonding of plastics, rubbers and metals. The transparent adhesive delivers rapid fixture times through moisture-activated curing and develops high bond strength on a wide range of substrates. Its higher viscosity enables better control during application while maintaining the fast-curing performance expected from cyanoacrylate technology. LOCTITE 416 also meets the lot requirements of Military Specification Mil-A-46050C and is qualified to Commercial Item Description A-A-3097, making it suitable for industrial assembly, maintenance and repair applications.

Key Features & Benefits

  • High-viscosity ethyl cyanoacrylate formulation.
  • One-component adhesive requiring no mixing.
  • Fast humidity-activated room-temperature cure.
  • Bonds plastics, rubbers and metals effectively.
  • Transparent cured bondline appearance.
  • Qualified to Mil-A-46050C and A-A-3097 specifications.
  • Excellent chemical and environmental resistance after cure.

Recommended Applications

  • General-purpose industrial bonding.
  • Plastic and rubber component assembly.
  • Metal-to-metal and mixed-material bonding.
  • Maintenance and repair operations.
  • High-strength precision assembly applications.

Technical Specifications

General Properties
Appearance Appearance
Transparent clear liquid
Specific Gravity Specific Gravity
1.05
Physical Properties
Viscosity Viscosity
1,150 - 1,500 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Ethyl cyanoacrylate adhesive
Chemical Type Ethyl Cyanoacrylate — General purpose instant adhesive
Appearance Transparent Clear Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.05 — 25°C
Viscosity (Cone & Plate) 900 - 1,500 mPa·s (cP) 100 s⁻¹, 25°C
Brookfield Viscosity 1,150 - 1,500 mPa·s (cP) LVF, Spindle 2, 12 rpm
Key Substrates Plastics, Rubbers and Metals — Typical bonding applications
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/m·K ISO 8302
Softening Point 165 °C DIN EN 1427
Volume Resistivity 2 × 10¹⁵ to 10 × 10¹⁵ Ω·cm IEC 60093
Surface Resistivity 10 × 10¹⁵ to 80 × 10¹⁵ Ω IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Lap Shear Strength (Steel) 18 - 26 N/mm² ISO 4587, Grit Blasted Steel
Lap Shear Strength (Aluminum) 12 - 19 N/mm² ISO 4587, Etched Aluminum
Tensile Strength (Steel) 12 - 25 N/mm² ISO 6922
Tensile Strength (Buna‑N) ≥6.0 N/mm² ISO 6922, 10 s Cure @ 22°C
T-Peel Strength (Steel) <0.5 N/mm ISO 11339