LOCTITE 348

Main features

  • Room-Temperature Adhesive Cure
  • Non-Sag Placement Control
  • Hand-Mixable Bonding Material

Product Description

LOCTITE® 348™ is a one-component, solvent-free epoxy adhesive supplied in convenient stick form for bonding, rebuilding, repairing and sealing applications. The hand-kneadable formulation combines resin and hardener in a single package and cures at room temperature after mixing. LOCTITE 348 adheres to a wide variety of substrates including metals, ceramics, wood, concrete and many rigid plastics, providing a durable bond with good mechanical strength and chemical resistance. Its non-sag consistency makes it particularly suitable for filling cracks, repairing damaged components and performing maintenance tasks in industrial environments.

Key Features & Benefits

  • Hand-mixable epoxy adhesive supplied in convenient stick form.
  • Ideal for repairing, rebuilding, filling and bonding applications.
  • Adheres to metals, wood, ceramics, concrete and many rigid plastics.
  • Non-sag consistency suitable for vertical and overhead repairs.
  • Room-temperature curing without specialized equipment.
  • Good chemical resistance and mechanical durability after cure.
  • Suitable for maintenance, repair and industrial service applications.

Recommended Applications

  • Repair of damaged equipment and machinery.
  • Filling cracks, voids and surface defects.
  • Bonding metal, concrete, ceramic and wood components.
  • Maintenance and emergency repair operations.
  • Rebuilding worn surfaces and damaged parts.
Product Family

LOCTITE 348

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g) Density (g)
1.3 g/cm3
Specific Gravity Specific Gravity
1.2
Physical Properties
Viscosity Viscosity
1000 - 5,000 mPa.s
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.25 W/m.K

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Epoxy — Two-part epoxy stick
Appearance Putty Stick — Before mixing
Color Off-White — Uncured
Mix Ratio 1:1 By Volume Integrated stick design
Working Time Approximately 3 min 23°C
Fixture Time Approximately 10 min Typical room-temperature cure
Full Cure Time 24 h 23°C
Application Form Hand Kneadable Putty — Maintenance repair use
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Compressive Strength 55 MPa Fully cured
Tensile Strength 6.9 MPa Room-temperature cure
Shore Hardness 85 Shore D Fully cured
Service Temperature Range -30 to 120 °C Typical operating conditions
Machinability Excellent — Can be drilled, tapped and sanded
Chemical Resistance Good — Resistant to many industrial fluids
Gap Filling Capability Excellent — Repair and rebuilding applications
Cured Material Type Rigid Epoxy Composite — After complete cure