LOCTITE 3341

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 3341 LOCTITE 3341

Main features

  • Fast UV/Visible-Light Fixturing
  • Flexible Plastic Bonding
  • UV-Fluorescent Presence Inspection

Product Description

LOCTITE AA 3341 is a one-component, low-viscosity acrylated urethane adhesive for UV/visible-light bonding and potting. It is formulated primarily for heavily plasticized PVC and also bonds polycarbonate and ABS. The transparent light-yellow liquid requires no mixing, fluoresces under UV light for presence inspection, and develops fixture strength in about 5 seconds under the specified 365 or 405 nm light conditions. After cure, the flexible material has 220% elongation and a 6.2 N/mm^2 block-shear result on polycarbonate-to-PVC assemblies at the stated cure condition. Applications include plastic bonding and disposable medical-device assembly.

Key features

  • Fast Light Fixture: Fixture strength develops in about 5 seconds under several listed 365 or 405 nm exposure conditions.
  • Flexible Cured Bond: A 220% elongation value provides a flexible cured material under the specified cure.
  • UV-Fluorescent Inspection: Positive UV fluorescence aids visual confirmation of adhesive presence.

Applications / Suitable for

  • Bonding heavily plasticized PVC
  • Bonding polycarbonate and ABS
  • Disposable medical-device assembly

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Acrylated urethane
Color Color
Transparent light yellow liquid
Component System Component System
One component
Refractive index Refractive index
1.5
Specific Gravity Specific Gravity
1.09
Physical Properties
Tack-Free Time Tack-Free Time
15 seconds minutes
Viscosity Viscosity
525 mPa.s
Chemical Properties
Water Absorption Water Absorption
3.64 %
Mechanical Properties
Elongation Elongation
220 %
Electrical Properties
Dielectric Strength Dielectric Strength
31.5 kV/mm
Volume Resistivity Volume Resistivity
9.62×10^14 Ohms⋅cm
Physical Properties
Depth of Cure Depth of Cure
4 mm
Curing Conditions
Fixture Time Fixture Time
15 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent light yellow-Uncured
UV fluorescencePositive-Uncured material under UV light
Specific gravity1.09-25 deg C
Viscosity525mPa sBrookfield RVT, spindle 1, 10 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Shore hardness27Durometer DISO 868; cured 30 seconds at 30 mW/cm^2 and 400 nm
Elongation at break220%ISO 527-3; same cure
Tensile strength at break15N/mm^2ISO 527-2; same cure
Tensile modulus25N/mm^2ISO 527-3; same cure
Block shear strength6.2N/mm^2ISO 13445; polycarbonate to PVC; same cure
Dielectric breakdown strength31.5kV/mmCured material

Leading Brands Trust in Our Products and Services