LOCTITE 190017

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 190017

Main features

  • Anaerobic Adhesive Technology
  • Above 100 deg C Flash Point
  • Clear Liquid Formulation

Product Description

LOCTITE 190017 1L EN is a clear, liquid anaerobic adhesive formulated for bonding and locking applications where curing occurs in the absence of air between closely fitting metal surfaces. The product exhibits a mild acrylic odor, a density of approximately 1.23 g/cm³, and a flash point greater than 100°C. Its liquid consistency supports dispensing and application in threaded assembly and retaining operations where anaerobic adhesive technology is commonly used. The material is supplied as a clear liquid and remains stable under recommended storage conditions. It is classified as a skin sensitizer and should be handled using appropriate industrial hygiene and personal-protection practices.

Key features

  • Anaerobic adhesive technology: Designed to cure in the absence of air for locking and bonding applications.
  • High flash point: Flash point greater than 100°C supports safer handling compared with lower-flash-point materials.
  • Clear liquid formulation: Liquid delivery form supports controlled dispensing during assembly operations.

Technical Specifications

General Properties
Density (g) Density (g)
1.17 g/cm3
Physical Properties
Viscosity Viscosity
5,000 - 9,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Physical properties of LOCTITE 190017 1L EN in its supplied liquid state.

Property Value Unit Method / condition
Technology Anaerobic adhesive — Product classification
Appearance Clear liquid — Delivery form
Density 1.2301 g/cm³ 20°C
Flash point >100 °C Tagliabue closed cup
Kinematic viscosity >20.5 mm²/s 40°C
Initial boiling point >150 °C Physical property