LINQSOL EMC-7535 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

EMC-7535 | Black Epoxy Mold Compound

Main features

  • Green molding compound
  • Designed for high-power TO packages
  • High Tg, low water absorption, low modulus, and excellent thermal stability

Product Description

LINQSOL EMC-7535 is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 175 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating,  EMC-7535 guarantees strong performance and outstanding reliability.

Overall, LINQSOL EMC-7535 seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages.

Product Family

LINQSOL EMC-7535

1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type, Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
black
Filler Content Filler Content
75 %
Specific Gravity Specific Gravity
1.96
Electrical Properties
Volume Resistivity Volume Resistivity
16000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption Moisture absorption
0.25 %
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
86 cm
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
175 °C
UL 94 Rating UL 94 Rating
V-0
Mechanical Properties
Molded Shrinkage Molded Shrinkage
0.1 %
Curing Conditions
Transfer Pressure Transfer Pressure
40-90 kg/cm2
Transfer Time Transfer Time
10-25 s

Additional Information

Processing Instructions

  • Before use, let LINQSOL EMC-7535 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 
  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7535 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers