LINQSEAL GS-VMQ

Harmonization Code : 4016.93 | Gaskets, washers and other seals made from vulcanized rubber

LINQSEAL VMQ

Main features

  • High flexibility
  • Wide temperature stability (–50 °C to 210 °C)
  • Good ozone and weather resistance

Product Description

LINQSEAL GS-VMQ gaskets are made from silicone rubbers with flexible siloxane (Si–O–Si) backbones. Vinyl methyl silicone rubbers contain vinyl (−CH=CH2) in addition to methyl groups (–CH3) in the most common silicone rubber (polydimethylsiloxane). This structure offers good flexibility, resistance to water and chemicals, and sealing performance. LINQSEAL GS-VMQ possesses excellent resistance to extreme temperatures from –55 °C to  210 °C. It also exhibits low compression sets, meaning it maintains its shape and sealing properties over time, ensuring reliable performance throughout the operational life of the system. 

Custom LINQSEAL GS-VMQ gaskets can be tailored precisely to your specifications and drawings. The thickness ranges from 0.5 to 5.0 millimeters. The maximum dimensions are 1500 × 1500 mm2, while the minimum dimensions are 100 × 100 mm2.

Key Features:

  • Outstanding low temperature flexibility
  • Excellent heat and oxidative stability
  • High temperature stability (–50 °C to 210 °C)
  • Low compression set
  • Hydrophobic

Highly Recommended As:

Product Family

LINQSEAL GS-VMQ

1. Select Package Type
2. Select Thickness

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature Operating Temperature
–50 to 210 °C
Mechanical Properties
Elongation Elongation
350 %

Additional Information

LINQSEAL GS-VMQ Flat Gasket Properties

Property Value Unit
Density 1.25–1.30 g/cm3
Tensile Strength 6 MPa
Elongation at Break 350 %
Hardness 65–70 Shore A
Operating Temperature –50 to 210 °C

 