LINQSEAL GS-PTFE

Harmonization Code : 4016.93 | Gaskets, washers and other seals made from vulcanized rubber

LINQSEAL PTFE

Main features

  • Outstanding chemical resistance
  • Wide temperature stability (–180 °C to 260 °C)
  • Excellent thermal and electrical resistance

Product Description

LINQSEAL GS-PTFE gaskets are made from a synthetic fluoropolymer of tetrafluoroethylene, known for its exceptional properties. The C–F bond within its polymer structure imparts inherent hydrophobicity, rendering PTFE ideal for applications requiring resistance to moisture and water-based substances. Moreover, PTFE boasts outstanding dielectric properties and remarkable temperature stability, ranging from –180 °C to 260 °C. Its unparalleled chemical resistance extends to acids, bases, and solvents. PTFE exhibits one of the lowest coefficients of friction against any solid, ensuring effective sealing and prolonged service life even in the most challenging environments. With all these exceptional properties, LINQSEAL GS-PTFE gaskets are widely used in industries requiring robust sealing solutions, including but not limited to automotive, aerospace, and manufacturing sectors.

Custom LINQSEAL GS-PTFE gaskets can be tailored precisely to your specifications and drawings. The thickness ranges from 0.5 to 5.0 millimeters. The maximum dimensions are 1500 × 1500 mm2, while the minimum dimensions are 100 × 100 mm2.

Key Features:

  • Outstanding chemical resistance
  • High electrical resistance
  • High temperature stability (–180 °C to 260 °C)
  • High resistance to creep under load or compression set
  • Hydrophobic and non-corrosive

Highly Recommended As:

 

Product Family

LINQSEAL GS-PTFE

1. Select Package Type
2. Select Thickness

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

LINQSEAL GS-PTFE Flat Gasket Properties

Property Value Unit
Density 2.10–2.30 g/cm3
Color White –
Compressibility 21 %
Tensile Strength 21–28 MPa
Elongation at Break 150 %
Leakage Rate 0.60×10–3 –
Dielectric Strength 10 kV/mm