LINQSEAL GS-EPDM

Harmonization Code : 4016.93 | Gaskets, washers and other seals made from vulcanized rubber

LINQSEAL EPDM

Main features

  • Low cost sealing solution
  • High hear resistance and tensile strength
  • High water (steam) resistance

Product Description

LINQSEAL GS-EPDM gaskets consist primarily of ethylene (comprising 45–75%), along with propylene and diene monomers. This unique composition provides the gaskets with exceptional versatility and durability. The diene monomers contribute to the formation of a cross-linking structure, enhancing the mechanical properties, such as elasticity, and significantly increasing resistance to aging. This rubber material exhibits high resistance to a wide range of environmental factors, including heat, cold, ozone, steam, electricity, UV rays, abrasion, and water, making it a preferred choice for various outdoor and challenging conditions. Compared to silicone and other polymers, EPDM boasts a higher tensile strength. Overall, LINQSEAL GS-EPDM is a cost-effective solution with outstanding performance in demanding outdoor environments.

Custom LINQSEAL GS-EPDM gaskets can be tailored precisely to your specifications and drawings. The thickness ranges from 0.5 to 5.0 millimeters. The maximum dimensions are 1500 × 1500 mm2, while the minimum dimensions are 100 × 100 mm2.

Key Features:

  • High tensile strength
  • High abrasion and weather resistance
  • Good temperature stability (–57 °C to 150 °C)

Highly Recommended As:

 

Product Family

LINQSEAL GS-EPDM

1. Select Package Type
2. Select Thickness

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g) Density (g)
1.45–1.50 g/cm3
Thermal Properties
Operating Temperature Operating Temperature
–57 to 150 °C
Mechanical Properties
Elongation Elongation
200 %