LINQBOND LB-DM801 | Dam encapsulant

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LINQBOND LB-DM801 | Dam encapsulant

Main features

  • Dam Encapsulant
  • Low CTE
  • High thixotropic index

Product Description

LINQBOND LB-DM801 is a high-performance, one-component epoxy adhesive specifically designed to work in conjunction with LB-FL501 as a dam material for semiconductor packaging. Together, these products provide a comprehensive solution for encapsulating and protecting electronic components.

With its low thermal expansion coefficient (CTE1: 20 ppm/°C, CTE2: 60 ppm/°C), LB-DM801 effectively prevents fill materials from spreading, ensuring precise control of encapsulant placement. Its thixotropic nature (TI: 3.1) and viscosity of 41800 cps at 25°C provide excellent sag resistance and dimensional stability, even on vertical surfaces.

Cure Schedule

  • 40 minutes @ 150°C
  • 20 minutes @ 160°C
Product Family

LINQBOND LB-DM801

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
139 °C
Physical Properties
Thixotropic index Thixotropic index
3.1
Viscosity Viscosity
42000 mPa.s