PTFE5S | 5-mil Skived PTFE Tape with Silicone Adhesive

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

5-mil Skived PTFE Tape Silicone Adhesive Single-Sided

Main features

  • 5 mil Skived PTFE film
  • Silicone adhesive
  • >13000V breakdown voltage

Product Description

LINQTAPE PTFE5S-Series describes our 5-mil thick Skived PTFE Film with a silicone pressure-sensitive adhesive. PTFE5S-Series tapes are used for high-temperature applications. They have excellent acid resistance as well as alkali resistance and have very low surface friction, making them ideal for heating panels. These tapes provide an excellent balance of electrical, thermal, and chemical properties over a wide range of temperatures, and can be used in applications that may see temperatures up to 260°C (500°F).

Further, PTFE5-Series have been used successfully to wrap high voltage wire in high-temperature operating conditions. Because of its Class H rating, it can be used in many electrical insulation applications. PTFE5S comes in 33-meter (36-yard) rolls of varying widths. LINQTAPE PTFE films with silicone adhesive are available in a range of thicknesses, starting from 2 mil (50.8µm) thickness and up. Custom thicknesses are available upon request.

 

Key Features:

  • Insulating tape
  • Pressure-sensitive silicone adhesive
  • High-temperature applications
  • Excellent acid and alkali resistance
  • Low surface friction
  • Class H rating
Product Family

LINQ PTFE5S

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Silicone
Adhesive Thickness Adhesive Thickness
38.1 µm
Chemistry Type Chemistry Type
PTFE
Color Color
Grey
Film Thickness Film Thickness
127.0 µm
Release Liner Release Liner
None
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single-Sided
Special Layer Special Layer
None
Total Thickness Total Thickness
165.1 μm
Thermal Properties
Temperature Resistance Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
>13000 V
Dielectric Strength Dielectric Strength
511 kV/mm
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
25 Oz/in
Elongation Elongation
300 %

Additional Information

Application Ideas

  • Heating panels
  • Electrical insulation
  • Thermal insulation
  • Wrapping and connecting high-voltage cables
  • Bellows and hose liners
  • Tank and vessel lining
  • Slide bearings