PIT2A-WL | 2-mil Polyimide (Kapton) Tape with Acrylic Adhesive | White-Labeled

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

2-mil Polyimide (Kapton) Tape Acrylic Adhesive White-Labeled 2-mil Polyimide (Kapton) Tape Acrylic Adhesive White-Labeled 2-mil Polyimide (Kapton) Tape Acrylic Adhesive White-Labeled 2-mil Polyimide (Kapton) Tape Acrylic Adhesive White-Labeled

Main features

  • 2 mil polyimide film
  • Non-silicone, acrylic adhesive
  • White-labeled

Product Description

LINQTAPE PIT2A-WL-Series is a Kapton Tape Alternative used for thermal printing and provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that require themal printing on parts that can see high temperatures such as steel or other alloys.

Product Family

LINQ PIT2A-WL

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Acrylic
Adhesive Thickness Adhesive Thickness
38.1 µm
Chemistry Type Chemistry Type
Polyimide
Color Color
White
Film Thickness Film Thickness
50.8 µm
Release Liner Release Liner
Kraft
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single-Sided
Special Layer Special Layer
Thermal Ink Print Layer
Total Thickness Total Thickness
88.9 μm
Thermal Properties
Temperature Resistance Temperature Resistance
300 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
11,000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
25 Oz/in
Elongation Elongation
60 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
88 N/cm