PIT2A-LO | 2-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT2A-LO | 2-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Main features

  • 2 mil polyimide film
  • Non-silicone, low outgassing acrylic adhesive
  • 6,500 V breakdown voltage

Product Description

LINQTAPE™ PIT2A-LO is a Polyimide tape with 2mil backing thickness and 1.5mil acrylic adhesive with low outgassing. This tape has less than 1% TML and less than 0.1% CVCM values, making it suitable for aerospace applications. 

LINQTAPE™ PIT2A-LO has good adhesion and tensile strength and can operate in temperatures between -29°C to 177°C.

Product Family

LINQ PIT2A-LO

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature Resistance Temperature Resistance
177 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
6,500 V
Mechanical Properties
Adhesion Strength Adhesion Strength
50 Oz/in
Elongation Elongation
55 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
88 N/cm
General Properties
Adhesive Layer Adhesive Layer
Low Outgassing Acrylic
Adhesive Thickness Adhesive Thickness
38.1 µm
Color Color
Amber
Film Thickness Film Thickness
50.8 µm
Release Liner Release Liner
Paper
Total Thickness Total Thickness
88.9 μm