PIT1S-UT-RL | 1mil Polyimide (Kapton) Tape | Ultra Thin Silicone Adhesive with Release Liner

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1S-UT-RL | 1mil Polyimide (Kapton) Tape | Ultra Thin Silicone Adhesive with Release Liner

Main features

  • 1 mil polyimide film
  • Ultra thin Silicone adhesive
  • >6000V breakdown voltage

Product Description

LINQTAPE™ PIT1S-UT-RL is a balanced, very thin and adjustable tape. It combines our 1-mil (25.4 micron) thick polyimide film – the generic equivalent of DuPont® Kapton™ HN tape – with an ultra thin 0.5mil (12.7 micron) silicone pressure adhesive and a release liner. This combination makes the PIT1S-UT-RL a very thin film with great breakdown voltage and a total thickness of only 1.5 mil (38.1µm). A product with excellent adhesion and electrical strength at high temperatures.

LINQTAPE™ PIT1S-UT-RL tapes are high performance, temperature resistant polyimide tapes that use a polyimide film as a backing film. This backing film is the generic version of DuPont's Kapton HN film and is thin at 1mil (25.4µm) yet is just as flame retardant as its thicker counterparts. Laminated to this is a 0.5mil (12.7µm) thick pressure sensitive silicone adhesive making the total thickness of the polyimide film plus adhesive only 1.5mil (38.1µm) thick. PIT1S-UT-RL remains both electrically and mechanically stable across temperatures ranging from -269°C to 400°C (-452°F to 752°F).

Polyimide tape is widely used in applications requiring high electrical insulation and an excellent balance of thermal, mechanical, chemical and electrical properties. As a base material, polyimide is extremely versatile as it can be die-cut, punched and thermoformed with or without adhesive.

It is extremely well suited, and extensively used for wrapping cable and magnet wire. A further list of applications includes, but is not limited to aircraft and spacecraft wiring, insulation tubing, slot insulation, fiber optics cable, heater circuits, automotive diaphragms and manifolds, high temperature splicing and other applications that can make use of the ultra-thin, high temperature, electrically insulating properties of the PIT1S-UT-RL polyimide HN tapes.

Applications

  • Cable Wrapping
  • Magnet Wire Wrapping
  • Automotive Manifolds
  • Automotive Diaphragms
  • Flexible Printed Circuits
  • Heater Circuits
  • Aircraft / Spacecraft Wiring
  • Insulation Tubing
  • Slot Insulation
  • Fiber Optics Cable
  • High Temperature Splicing
  • 3D printing ABS plastic

Product Features and Benefits

  • Good Chemical Resistance
  • Mechanically and electrically stable from -269°C to 400°C (-452°F to 752°F)
  • Can be laminated, die-cut, metallized, punched, adhesive coated and thermoformed
  • Insensitive to radiation damage
  • Adheres well to ABS
  • Improved Moiture Barrier

Product Nomenclature

  • PIT: HN Polyimide Tape
  • 1: 1 mil (25.4µm) thick tape
  • S: Silicone adhesive
  • UT: 0.5 mil Thin Adhesive Layer
  • RL: Release liner
Product Family

LINQ PIT1S-UT-RL

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Silicone
Adhesive Thickness Adhesive Thickness
12.7 µm
Chemistry Type Chemistry Type
Polyimide
Color Color
Amber
Film Thickness Film Thickness
25.4 µm
Release Liner Release Liner
Yes
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single-Sided
Special Layer Special Layer
None
Total Thickness Total Thickness
38.1 μm
Thermal Properties
Temperature Resistance Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
>6000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
8 Oz/in

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers