PIT1S-ESD | 1-mil Antistatic ESD Polyimide (Kapton) Tape with Silicone Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

1-mil Antistatic ESD Polyimide (Kapton) Tape Silicone PIT1S-ESD | 1-mil Antistatic ESD Polyimide (Kapton) Tape with Silicone Adhesive

Main features

  • 1 mil polyimide film
  • Silicone adhesive
  • >6,500V breakdown voltage

Product Description

LINQTAPE™ PIT1S-ESD Series is a high-temperature resistant, antistatic-treated polyimide film mounted with a silicone adhesive. It is designed for both masking and temporary bonding in many high-temperature applications in semiconductor, electronic, automotive, and other general manufacturing industries.

LINQTAPE™ PIT1S-ESD Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 260°C (500°F).

LINQTAPE™ PIT1S-ESD Series comes as a standard in 36-yard (33m) lengths of varying widths, but longer rolls may be available upon request.

 

Key Features:

  • Antistatic coating to dissipate electrostatic charge
  • Pressure-sensitive silicone adhesive
  • Excellent insulating properties
Product Family

LINQ PIT1S-ESD

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature Resistance Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
6500 V
General Properties
Adhesive Layer Adhesive Layer
Silicone
Adhesive Thickness Adhesive Thickness
38.1 µm
Chemistry Type Chemistry Type
Polyimide
Color Color
Amber
Film Thickness Film Thickness
25.4 µm
Release Liner Release Liner
None
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single-Sided
Special Layer Special Layer
Antistatic Polymer Coating
Total Thickness Total Thickness
63.5 μm
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
25 Oz/in
Elongation Elongation
55 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
52 N/cm

Additional Information

Application Ideas

  • Dissipate electrostatic charges
  • Ideal for wafer dicing and die-cutting
  • Temporary bonding of thermocouples for oven profiling
  • Bonding of devices before solder reflow
  • Splicing of insulation layers