PIT1S-B | 1-mil Black Polyimide (Kapton) tape with Silicone Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1S-B | 1-mil Black Polyimide (Kapton) tape with Silicone Adhesive

Main features

  • 1 mil polyimide Film
  • Opaque black color through the film
  • 3000V Breakdown Voltage

Product Description

LINQTAPE PIT1S-B is a Kapton HN Alternative whose high performance, flexible, high-temperature resistant polyimide film is used for many high-temperature applications. Polyimide is preferred over polyester for many high-temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive, and general manufacturing industries.

LINQTAPE PIT1S-B Tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. Tapes are typically only limited by their adhesive. This Silicone tape can be used in applications up to 260°C. This PIT1S-B(lack) film has an opaque black coloring, which results in almost no light transmission, higher heat resistance and higher resistivity than the standard PIT1S.

Product Family

LINQ PIT1S-B

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Silicone
Color Color
Black
Film Thickness Film Thickness
25.4 µm
Thermal Properties
Temperature Resistance Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
3000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
25 Oz/in
Elongation Elongation
55 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
338 N/cm