PIT0.5N-DCD | 0.5 mil Die Cut Polyimide (Kapton) Film| Single Sided Discs

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT0.5N-DCD | 0.5 mil Die Cut Polyimide (Kapton) Film| Single Sided Discs

Main features

  • 0.5 mil polyimide film
  • No adhesive
  • Die cut discs

Product Description

LINQTAPE PIT0.5N-DCD is a 0.5-mil, Kapton HN Film without any adhesive whose high performance, flexible, high-temperature resistant polyimide films used for many high temperature applications. Polyimide is preferred over polyester for many high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE PIT0.5N-DCD Series Film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 400°C (752°F).

LINQTAPE PIT0.5N-DCD polyimide tape can be delivered in a range of die cut discs sizes with diameters ranging from 1/8" to 12".

Product Family

LINQ PIT0.5N-DCD

1. Select Diameter

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Diameter.

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
None
Chemistry Type Chemistry Type
Polyimide
Color Color
Amber
Film Thickness Film Thickness
12.7 µm
Release Liner Release Liner
None
Special Layer Special Layer
None
Total Thickness Total Thickness
12.7 μm
Thermal Properties
Temperature Resistance Temperature Resistance
400 ˚C
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Elongation Elongation
>35 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
20,000 N/cm
Electrical Properties
Breakdown Voltage Breakdown Voltage
>3000 V

Leading Brands Trust in Our Products and Services