PIT0.5N | 0.5-mil Polyimide (Kapton) Film

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT0.5N | 0.5-mil Polyimide (Kapton) Film

Main features

  • 0.5 mil polyimide film
  • No adhesive
  • >3000V breakdown voltage

Product Description

LINQTAPE PIT0.5-Series is a high-temperature resistant polyimide film designed for both permanent and temporary bonding in many high-temperature applications. These applications can be found in semiconductor, smartcard,
electronic, automotive, and general manufacturing industries. It is ideal for applications that require the balancing of multiple properties over a wide temperature range. LINQTAPE PIT0.5-Series film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 400°C.

LINQTAPE™ PIT0.5N Film comes in 33-meter (36-yard) rolls of varying widths. LINQTAPE PIT-N polyimide films without adhesive are available in a range of thicknesses, starting from 0.5 mil (12.7µm) thickness and up. Custom thicknesses are available upon request.

Key Features:

  • High-temperature applications
  • Thin film without adhesive
  • Excellent electrical properties
Product Family

LINQ PIT0.5N

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
None
Chemistry Type Chemistry Type
Polyimide
Color Color
Amber
Film Thickness Film Thickness
12.7 µm
Special Layer Special Layer
None
Total Thickness Total Thickness
12.7 μm
Thermal Properties
Temperature Resistance Temperature Resistance
400 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
>3000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Elongation Elongation
>35 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
20,000 N/cm