PET2S-Blue-DCD | 2-mil Blue Die Cut Polyester (PET) Tape with Silicone Adhesive | Single-Sided Discs

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

2-mil Blue Die Cut Polyester (PET) Tape Acrylic Adhesive Single-Sided | Discs

Main features

  • 2 mil die cut polyester film
  • Silicone adhesive
  • 7000V breakdown voltage

Product Description

LINQTAPE PET2S is a 2-mil polyester film backing with a pressure sensitive silicone adhesive system. PET2S polyester tape is a no/low residue tape designed for splicing and masking applications where high initial adhesion is required, but no residue once the tape is removed.

LINQTAPE PET2S is a high performance, flexible, polyester tape used in a wide range of applications. For very high temperature applications, polyimide tape should be used, but for applications with temperatures up to 200C PET2S is the most effective and least expensive solution. PET2S-DCD polyester tape can be delivered in a range of die cut discs sizes with diameters ranging from 1/8" to 12".

 

Key Features:

  • No residue
  • High initial adhesion
  • For splicing and masking
  • High performance
  • Flexible
Product Family

LINQ PET2S-Blue-DCD

1. Select Diameter

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Diameter.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Silicone
Adhesive Thickness Adhesive Thickness
38.1 µm
Chemistry Type Chemistry Type
Polyester
Color Color
Blue
Film Thickness Film Thickness
50.8 µm
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single sided
Total Thickness Total Thickness
88.9 μm
Thermal Properties
Temperature Resistance Temperature Resistance
200 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
7000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
VOC-Free (100% solids content) VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
30 Oz/in
Elongation Elongation
100 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
88 N/cm