OLS-1557 | Liquid Encapsulant - Two part Epoxy

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OLS-1557 | Liquid Encapsulant - Two part Epoxy

Main features

  • Low viscosity
  • Good workability
  • High temperature resistance

Product Description

OPTOLINQ OLS-1557 is an optically clear, two-part, and heat-curable epoxy resin. OLS-1557 AB mixture has low viscosity and good workability after mixing. When fully cured, the product demonstrates minimal mold shrinkage, high toughness, high-temperature resistance, good adhesion on different surfaces, and excellent electrical properties, making OLS-1557 an ideal material for the encapsulation of optoelectronic devices. 

 

Product Family

LINQ OLS-1557

1. Select Package Type
2. Select Weight

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type and Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C Work life @25°C
4 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
81–91 °C
Chemical Properties
Water Absorption Water Absorption
0.3 %

Additional Information

Processing Instructions

  • Mix component A and B, stir uniformly, and degas under vacuum. 
  • Recommended molding curing conditions: Mold at 150 °C for 5 minutes and post-mold cure at 130–135 °C for 6–8 hours. Identify the specific curing settings based on your product requirements.

Using Additives

Optolinq OLS-1557 can be mixed with diffusing agents or color pastes to achieve customer-specific purposes.

Recommended quantity of various diffusing agents and color pastes:

  • OPC-R Red Color Paste: 0.1-0.5% by epoxy weight
  • OPC-B Blue Color Paste: 0.1-0.5% by epoxy weight
  • OPC-G Green Color Paste: 0.1-0.5% by epoxy weight
  • ODF-090 Diffusing Agent: 3-5% by weight (LED lamps), 4-8% (LED displays)

Storage and Handling

Store in a ventilated, dry, and clean environment below 30 °C and  70% RH. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A has a shelf life of 6 months and Part B a shelf life of 3 months. Shelf life can be extended by using cold storage.