LINQSOL EMC-G836 is a halogen-free epoxy molding compound engineered for the precise encapsulation of a wide range of semiconductor packages, including Quad Flat No-Leads (QFN), Quad Flat Packages (QFP), and other thin, high-density packages like BGA TF cards (microSD). Its design focuses on delivering both superior performance and exceptional reliability.

Product Key Features

  • Wide gel time (36s) — offers a broader processing window, ideal for QFN and QFP molding applications.
  • High spiral flow (149cm) — meets demanding flowability requirements for intricate package designs.
  • Low water absorption
  • RoHS and REACH compliant

Applications

  • Encapsulation of quad flat no-leads (QFN) & quad flat packages (QFP)
  • Encapsulation of thin, high-density packages, including BGA TF cards (microSD)
Product Family

LINQ EMC-G836

1. Select Pellet Size
2. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity Specific Gravity
2
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
149 cm
Viscosity Viscosity
18000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity Thermal Conductivity
0.92 W/m.K
UL 94 Rating UL 94 Rating
V-0

Additional Information

LINQSOL EMC-G836 Recommended Mold Parameters

Parameters Value Unit
Molding Temperature 170-180 ℃
Transfer Pressure 70-150 kgf/cm2
Transfer Time 8-25 s
Cure Time 100-180 s
Post Mold Cure Time 4-8 h