LAIRD TFLEX HD92000

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD TFLEX HD92000

Main features

  • 2.00 mm High-Deflection Interface
  • 7.5 W/mK Heat Transfer
  • 82% Deflection at 50 psi

Product Description

Tflex HD92000 High-Deflection Thermal Gap Filler is a 2.00 mm grey ceramic-filled silicone pad for compliant thermal contact across wider electronic assembly gaps. The HD90000 material provides 7.5 W/(m K) thermal conductivity with Shore 00 hardness of 32 and strong pressure-responsive deflection. At 10 psi, the 2.00 mm configuration has typical thermal resistance of 0.35 deg C-in2/W and 27% deflection; deflection reaches 82% at 50 psi. Applications include automotive electronics, portable devices, routers, instrumentation, gaming systems, and wireless infrastructure.

Key features

  • 2.00 mm High-Deflection Interface: The HD92000 configuration provides a 0.080 inch compliant thermal pad.
  • 7.5 W/(m K) Thermal Conductivity: Ceramic-filled silicone supports heat transfer across controlled component gaps.
  • Pressure-Responsive Conformability: Typical deflection increases from 27% at 10 psi to 82% at 50 psi.

Applications / Suitable for

  • Automotive and industrial electronic modules
  • Portable devices, routers, and gaming systems
  • Instrumentation and wireless infrastructure

Technical Specifications

General Properties
Color Color
Grey
Component System Component System
Ceramic filled silicone sheet
Density (g) Density (g)
3.5 g/cm3
Thermal Properties
Operating Temperature Operating Temperature
(-)65 to 125 °C
Thermal Conductivity Thermal Conductivity
7.5 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied HD90000 material properties for the 2.00 mm Tflex HD92000 configuration.

Property Value Unit Method / condition
Construction Ceramic-filled silicone sheet Tflex HD90000 series
Color Grey Visual
Nominal thickness 2.00 mm 0.080 inch product configuration
Density 3.50 g/cc Helium pycnometer
Hardness 32 Shore 00 ASTM D2240; 1000 um and above
Outgassing TML 0.170 % ASTM E595
Outgassing CVCM 0.010 % ASTM E595
Shelf life 1 year from shipment Typical series property
Technical properties

After-processing / final-state properties

Typical HD92000 thermal and deflection data at the stated pressures; installed results depend on surface contact and assembly compression.

Property Value Unit Method / condition
Thermal conductivity 7.5 W/(m K) Hot Disk
Thermal resistance at 10 psi 0.35 deg C-in2/W Typical 2.00 mm configuration
Thermal resistance at 30 psi 0.09 deg C-in2/W Typical 2.00 mm configuration
Thermal resistance at 50 psi 0.09 deg C-in2/W Typical 2.00 mm configuration
Deflection at 10 psi 27 % Typical 2.00 mm configuration
Deflection at 50 psi 82 % Typical 2.00 mm configuration
Operating temperature -65 to 125 deg C Current product page