Main features

  • Over 50% Deflection at 50 psi
  • 1.2 W/(m K) Thermal Conductivity
  • 0.50 to 5.08 mm Thickness Range

Product Description

Tflex™ 300 is a ceramic-filled silicone thermal gap filler designed to conform around components and bridge gaps between heat-generating devices and adjacent cooling surfaces. The light-green pad provides typical thermal conductivity of 1.2 W/m·K and deflects by more than 50% of its original thickness at 50 psi. Its low compression set supports repeated installation, while available thicknesses from 0.50 mm to 5.08 mm address a range of interface geometries. :contentReference[oaicite:0]{index=0}

Key features

  • Highly compliant construction: Deflects by more than 50% of its original thickness at 50 psi, supporting conformity around component topography.
  • Thermal gap-filling performance: Provides typical thermal conductivity of 1.2 W/m·K when tested according to ASTM D5470.
  • Broad thickness availability: Offered from 0.50 mm (0.020 in) to 5.08 mm (0.200 in), with standard and custom-converted formats available.

Applications / Suitable for

  • Automotive electronics, infotainment, ADAS, and powertrain or ECU assemblies
  • Routers and wireless infrastructure
  • Notebooks, tablets, portable devices, gaming systems, and smart-home devices
  • Instrumentation and drone or satellite electronics

Technical Specifications

General Properties
Color Color
Light Green
Component System Component System
Ceramic Filled Silicone Sheet
Density (g) Density (g)
1.78 g/cm3
Thickness range Thickness range
0.5 - 5.08 mm
Thermal Properties
Operating Temperature Operating Temperature
-40 to 160 °C
Thermal Conductivity Thermal Conductivity
1.2 W/m.K
Electrical Properties
Volume Resistivity Volume Resistivity
10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uninstalled properties and available dimensions for the Tflex 300 Series. Values are for design guidance and are not guaranteed specifications. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Construction and composition Ceramic-filled silicone sheet — Product construction
Color Light green — Visual
Thickness range 0.50–5.08 (0.020–0.200) mm (in) Nominal uncompressed thickness range
Density 1.78 g/cc Helium pycnometer
Hardness 51.4 for 20–30 mil
25.2 for 40 mil and above
Shore 00 ASTM D2240; thickness-dependent result
Shelf life 2 years From date of shipment; storage conditions not stated on the product page
Technical properties

After-processing / final-state properties

Typical thermal, electrical, environmental, and installed-interface properties of Tflex 300. Values are not intended as guaranteed design limits. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
Thermal conductivity 1.2 W/m·K ASTM D5470
Thermal resistance 0.98 °C·in²/W Modified ASTM D5470; 40 mil thickness, 10 psi, 50°C
Deflection >50 % At 50 psi; thickness-specific curves are provided in the datasheet
Operating-temperature range -40 to 160 °C Documented product temperature range
Dielectric constant 4.5 — ASTM D150 at 10 GHz
Volume resistivity 1013 ohm·cm ASTM D257
Outgassing TML: 0.56
CVCM: 0.10
wt% ASTM E595