LAIRD CRS-124

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD CRS-124

Main features

  • Flexible RTV Silicone Microwave Absorber
  • 100:1.00 Controlled Mixing
  • 1.0 W/(m K) Thermal Conductivity

Product Description

ECCOSORB™ CRS-124 Castable Silicone Absorber is a two-part, magnetically loaded RTV silicone microwave absorber that cures to a flexible elastomer. The CRS-124 grade uses a 100:1.00 Part A-to-Part B mix ratio and may be poured into cavities, cast into cones, wedges, pyramids, terminations, loads, or microwave gaskets, and shaped to contoured surfaces. The system cures overnight at room temperature or in three hours at 80°C. Typical cured properties include 1.0 W/m·K thermal conductivity, Shore A 75 hardness, low water absorption, and service below 160°C.

Key features

  • Flexible silicone absorber: The cured elastomer can be shaped to contoured surfaces and withstand impact or shock.
  • 1.0 W/m·K thermal conductivity: CRS-124 provides the higher thermal conductivity of the two CRS grades.
  • Pour-in-place processing: The material can form cavities, loads, gaskets, and custom absorber geometries.

Applications / Suitable for

  • Microwave terminations and loads
  • Pour-in-place microwave gaskets
  • Cavity filling and contoured absorber surfaces
Product Family

LAIRD CRS-124

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Two-part magnetically loaded RTV silicone N/A Part A and Part B
Part A form High-viscosity paste N/A As supplied
Mix ratio 100:1.00 parts by weight Part A : Part B
Shelf life Approximately 6 months At or below 25°C
Room-temperature cure Overnight N/A Documented schedule
Accelerated cure 3 h At 80°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Service temperature <160 °C Typical
Density 4.55 g/cm³ Typical
Coefficient of thermal expansion 59 × 10⁻⁶ 1/°C Typical
Thermal conductivity 1.0 W/m·K Typical
Hardness 75 Shore A Typical
Water absorption <0.1 % 24 h
Dielectric strength >10 V/mil Typical
Volume resistivity >1 × 10¹⁰ ohm·cm Typical