LAIRD CR-114

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD CR-114

Main features

  • 10 to 14 GHz Absorption Range
  • 100:6.5 Controlled Mixing
  • Below 180 deg C Service Temperature

Product Description

ECCOSORB™ CR-114 Castable Epoxy Absorber is a two-part, castable epoxy microwave absorber for molding waveguide terminations, attenuators, loads, and custom absorber shapes or for potting localized radio-frequency leakage. The CR-114 grade uses a 100:6.5 Part A-to-Part B mix ratio and is positioned for approximately 10 to 14 GHz. The material is processed warm to improve pourability and may be cured from 75°C to 150°C using the documented schedule. Shared CR-family properties include low outgassing, service below 180°C, low water absorption, and suitability for aerospace, defense, telecom, and test applications.

Key features

  • 10 to 14 GHz grade: CR-114 is positioned for microwave absorption within the documented frequency range.
  • Castable epoxy absorber: The system can mold terminations, attenuators, loads, and custom absorber shapes.
  • Low-outgassing family: The CR series is documented for low-outgassing applications.

Applications / Suitable for

  • Waveguide terminations and loads
  • Attenuators and custom absorber shapes
  • Localized RF-leakage potting
Product Family

LAIRD CR-114

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Two-part castable epoxy absorber N/A Part A and Part B
Color Dark gray N/A Product family
Mix ratio 100:6.5 parts by weight Part A : Part B
Recommended frequency range 10 to 14 GHz CR-114 grade
Pot life Approximately 30 min At 65°C
Cure options 12 h at 75°C; 4 h at 90°C; 2 h at 120°C; 1 h at 150°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Service temperature <180 °C CR family
Coefficient of thermal expansion 30 × 10⁻⁶ 1/°C CR family
Water absorption 0.1 % Seven-day immersion
Flexural strength 15,000 psi Typical CR-family value
Total mass loss 0.08 to 0.51 % ASTM E595
Collected volatile condensable material 0.001 to 0.01 % ASTM E595