INSULCURE 11B

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

INSULCURE 11B

Main features

  • Heat-Curing INSULCAST Epoxy Curing Agent
  • 700 cP Application Viscosity
  • 3-Hour 100 deg C Cure

Product Description

INSULCURE® 11B Epoxy Curing Agent is a rigid, temperature-resistant, heat-curing agent for compatible INSULCAST epoxy casting and encapsulation resins. The amber liquid is selected when extended pot life and elevated-temperature cured performance are required. Current supplier information lists a typical viscosity of 700 cP, a 300-minute pot life in the referenced system, and a three-hour cure schedule at 100°C. Final mix ratio and cured properties depend on the specific INSULCAST resin, so this component should be presented and processed only as part of a verified resin-hardener system.

Key features

  • Heat-curing epoxy hardener: The curing agent is intended for compatible INSULCAST resin systems.
  • Extended process window: Current supplier information lists a 300-minute pot life in the referenced system.
  • Temperature-resistant rigid cure: The product is positioned for elevated-temperature epoxy systems.

Applications / Suitable for

  • Curing compatible INSULCAST epoxy resins
  • Heat-cured electrical potting systems
  • Temperature-resistant epoxy casting systems
Product Family

INSULCURE 11B

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Epoxy curing agent N/A As supplied
Appearance Amber liquid N/A Product family description
Viscosity 700 cP Current supplier product page
Pot life 300 min Referenced system at 25°C
Reference cure 3 h At 100°C