INSULCAST RTVS A-4000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INSULCAST RTVS A-4000

Main features

  • Two-Component Solvent-Based Silicone Adhesive for Silicones
  • 900 to 2,500 cP Mixed Viscosity
  • 73 to 260 deg C Service Range

Product Description

INSULCAST® RTVS A-4000 Silicone Adhesive is a two-component, solvent-based silicone resin adhesive for bonding silicones, Mylar, metals, and selected engineering plastics. The light-straw Part A and clear Part B are mixed at 100:3.3 by weight to produce a typical mixed viscosity of 900 to 2,500 cP. The adhesive is documented for lap-shear and peel performance at elevated temperature and retains flexibility from -73°C to 260°C. It may cure for one to four days at room temperature or be accelerated with an eight-hour cure at 200°C.

Key features

  • Elevated-temperature bonding: The adhesive retains flexibility from -73°C to 260°C.
  • Silicone and film adhesion: Documented substrates include silicones, Mylar, metals, and engineering plastics.
  • Low mixed viscosity: Typical mixed viscosity is 900 to 2,500 cP.

Applications / Suitable for

  • Bonding silicone materials
  • Bonding Mylar and metal assemblies
  • High-temperature engineering-plastic bonding

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A color Light straw N/A As supplied
Part B color Clear N/A As supplied
Part A viscosity 1,000 to 5,000 cP At 25°C
Part B viscosity 50 cP At 25°C
Mix ratio 100:3.3 parts by weight Part A : Part B
Mixed viscosity 900 to 2,500 cP Typical
Pot life 24 min At 25°C
Solids content 55 % Part A
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Service temperature -73 to 260 °C Documented range
180° peel strength 36 oz/in Mylar-to-Mylar
Lap shear strength 130 psi Mylar-to-Mylar at 25°C
Lap shear strength 120 psi Silicone-to-aluminum at 25°C
Dielectric strength 450 V/mil ASTM D149
Room-temperature cure 1 to 4 days Documented schedule
Accelerated cure 8 h At 200°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers