INSULCAST RTVS 8128

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INSULCAST RTVS 8128

Main features

  • Low-Viscosity Encapsulation Application
  • 2,200 cP Mixed Viscosity
  • 55 to 204 deg C Service Range

Product Description

"

INSULCAST® RTVS 8128 Silicone Encapsulant is a dark-gray, two-component, low-viscosity, flame-retardant, reversion-resistant RTV silicone for general-purpose and high-voltage potting applications. The 1:1 system has a typical mixed viscosity of 2,200 cP and a 60 to 90-minute pot life at 25°C, followed by a 24-hour room-temperature cure. After cure, the silicone has Shore A 50 hardness, 0.31 W/m·K thermal conductivity, 550 V/mil dielectric strength, and service from -55°C to 204°C. Published portfolio data state that the product meets UL 94 V-0.

Key features

  • High-voltage potting: Typical cured dielectric strength is 550 V/mil.
  • Low-viscosity 1:1 system: Typical mixed viscosity is 2,200 cP.
  • Flame-retardant RTV protection: Published portfolio data state that the product meets UL 94 V-0.

Applications / Suitable for

  • High-voltage electronic potting
  • General-purpose electrical casting
  • Repairable silicone encapsulation

"

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color Dark gray N/A Mixed system
Mix ratio 1:1 ratio Part A : Part B
Mixed viscosity 2,200 cP Typical
Pot life 60 to 90 min At 25°C
Cure time 24 h At 25°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 50 Shore A Typical cured value
Thermal conductivity 0.31 W/m·K Typical cured value
Dielectric constant 3.0 N/A At 1 kHz
Dielectric strength 550 V/mil Typical cured value
Volume resistivity 1.5 × 10¹⁵ ohm·cm Typical cured value
Coefficient of thermal expansion 22 × 10⁻⁵ 1/°C Typical cured value
Service temperature -55 to 204 °C Documented range
Flammability classification Meets V-0 UL 94 Published portfolio statement