INSULCAST RTVS 8127

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

INSULCAST RTVS 8127

Main features

  • Flame-Retardant 1:1 Silicone Encapsulation
  • 4,000 cP Mixed Viscosity
  • 0.75 W/(m K) Thermal Encapsulation

Product Description

INSULCAST® RTVS 8127 Silicone Encapsulant is a gray, two-component, flame-retardant, reversion-resistant silicone compound for potting dense electronic packages that require heat dissipation. The 1:1 system has a typical mixed viscosity of 4,000 cP and a 160 to 220-minute pot life at 25°C, supporting controlled flow before a 24-hour room-temperature cure. After cure, the silicone has Shore A 55 hardness, 0.75 W/m·K thermal conductivity, 500 V/mil dielectric strength, and service from -55°C to 204°C. The product is documented as UL 94 V-0.

Key features

  • Thermally conductive silicone: Typical cured thermal conductivity is 0.75 W/m·K.
  • Long process window: Typical pot life is 160 to 220 minutes at 25°C.
  • Flame-retardant electrical protection: The product is documented as UL 94 V-0 with 500 V/mil dielectric strength.

Applications / Suitable for

  • Dense electronic package potting
  • Electronic assemblies requiring heat dissipation
  • Flame-retardant silicone encapsulation

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color Gray N/A Mixed system
Mix ratio 1:1 ratio Part A : Part B
Mixed viscosity 4,000 cP Typical
Pot life 160 to 220 min At 25°C
Cure time 24 h At 25°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 55 Shore A Typical cured value
Thermal conductivity 0.75 W/m·K Typical cured value
Dielectric constant 4.0 N/A At 1 kHz
Dielectric strength 500 V/mil Typical cured value
Volume resistivity 1 × 10¹⁵ ohm·cm Typical cured value
Coefficient of thermal expansion 18 × 10⁻⁵ 1/°C Typical cured value
Service temperature -55 to 204 °C Documented range
Flammability classification V-0 UL 94 Documented classification