INSULCAST 987

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

INSULCAST 987

Main features

  • Semi-Flexible Broad-Temperature Epoxy Potting
  • 60,000 cP Mixed Viscosity
  • -55 to 155 deg C Service Range

Product Description

INSULCAST® 987 Semi-Flexible Epoxy Potting Compound is a filled, semi-flexible, two-component epoxy potting compound for electrical and electronic assemblies operating across a broad temperature range. The neutral Part A and Part B are mixed at 2:3 by weight and produce a typical mixed viscosity of 60,000 cP with more than 48 hours of work life at 25°C. The system is heat cured and is documented for electrical insulation and physical durability. Typical cured properties include Shore D 65 hardness, 0.417 W/m·K thermal conductivity, 375 V/mil dielectric strength, and service from -55°C to 155°C.

Key features

  • Semi-flexible epoxy: The filled cured material combines Shore D 65 hardness with broad-temperature service.
  • Extended work life: Typical work life is greater than 48 hours at 25°C.
  • Electrical insulation: Typical cured dielectric strength is 375 V/mil with 1 × 10¹⁴ ohm·cm volume resistivity.

Applications / Suitable for

  • Electrical and electronic potting
  • Broad-temperature encapsulation
  • Heat-cured semi-flexible castings

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A color Neutral N/A As supplied
Part B color Neutral N/A As supplied
Part A viscosity 80,000 cP At 23°C
Part B viscosity 50,000 cP At 23°C
Mix ratio 2:3 parts by weight Part A : Part B
Mixed viscosity 60,000 cP Typical
Work life >48 h At 25°C
Cure options 2 h at 120°C; 24 h at 75°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 65 Shore D ASTM D2240
Coefficient of thermal expansion 45 × 10⁻⁶ 1/°C Typical cured value
Thermal conductivity 0.417 W/m·K Converted from 2.9 BTU-in/(ft²·h·°F)
Service temperature -55 to 155 °C Documented range
Dielectric strength 375 V/mil ASTM D149
Dielectric constant 4.9 N/A At 1 kHz
Dissipation factor 0.05 N/A At 1 kHz
Volume resistivity 1 × 10¹⁴ ohm·cm ASTM D257