INDIUM SMQ92J

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM SMQ92J

Main features

  • High-Speed Fine-Pitch Printing
  • Long Stencil and Tack Life
  • Probe-Testable No-Clean Residue

Product Description

Indium NC-SMQ92J No-Clean Solder Paste is a halogen-free, air-reflow solder paste for high-speed surface-mount assembly. The flux system supports consistent fine-pitch deposition, extended open time, strong initial tack, and more than 12 hours of stencil life under the stated conditions. It leaves a benign, probe-testable residue that can be penetrated by multi-point probes without clogging. A typical Sn63 Type 3 printing configuration has 2,000 poise viscosity and 38 g tackiness. Applications include fast-print SMT lines, rapid component placement, fine-pitch printing, and air or nitrogen reflow with the supported SnPb alloy configurations.

Key features

  • High-Speed SMT Printing: Supports fast print speeds and rapid component placement with consistent fine-pitch deposition.
  • Long Stencil and Tack Life: More than 12 hours of stencil life under stated conditions combines with strong initial tack.
  • Probe-Testable Residue: Benign residue is penetrated by multi-point probes without clogging.

Applications / Suitable for

  • High-speed SMT printing
  • Fine-pitch component placement
  • SnPb air or nitrogen reflow
Product Family

INDIUM SMQ92J

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life Stencil Life
More than 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for NC-SMQ92J; the specified Sn63 Type 3 printing configuration is identified where required.

Property Value Unit Method / condition
Flux classification ROL0 J-STD-004
Typical viscosity 2,000 poise Sn63, 90.25% metal load, Type 3; Malcolm at 10 rpm
Typical thixotropic index -0.75 SSF; ICA test
Typical tackiness 38 g J-STD-005 test result
Stencil life greater than 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C