INDIUM 10.8HF

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM 10.8HF

Main features

  • Broad Air-Reflow Process Window
  • Low-Voiding QFN and BGA
  • Halogen-Free ROL0 Flux System

Product Description

Indium10.8HF Pb-Free Solder Paste is a halogen-free, no-clean lead-free solder paste for surface-mount printing and air reflow. The ROL0 flux system supports broad lead-free process windows, high transfer efficiency, and controlled coalescence across Type 3, Type 4, Type 5, and T5-MC powder options. It is formulated for low voiding in QFN and BGA joints and leaves a clear residue after reflow. Under the stated shop conditions, stencil life extends up to 12 hours. Applications include lead-free SMT stencil printing and reflow where the ordered alloy, powder size, storage condition, and thermal profile are specified.

Key features

  • Broad Reflow Profile Window: The flux system supports lead-free air-reflow processing across documented profile conditions.
  • Low-Voiding QFN/BGA Reflow: The paste is formulated for low voiding in QFN and BGA solder joints.
  • Clear Post-Reflow Residue: The no-clean flux leaves a clear residue after the documented reflow process.

Applications / Suitable for

  • Lead-free SMT stencil printing
  • QFN and BGA assembly
  • Air reflow with the ordered alloy and powder configuration
Product Family

INDIUM 10.8HF

Loading pricing…

Technical Specifications

Other Properties
Stencil Life Stencil Life
Up to 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for Indium10.8HF; alloy, powder, package, storage, and environmental conditions are identified where they affect the value.

Property Value Unit Method / condition
Flux classification ROL0 IPC J-STD-004D
Typical viscosity 1,400 kcps Type 4 and Type 4.5 powder
Metal load 89 % Type 4 and Type 4.5 powder
Metal load 88.0 to 88.5 % Type 5 and T5-MC powder
Stencil life up to 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Syringe stored below -10 deg C
Shelf life 6 months Jar or cartridge stored below 10 deg C
Halogen limits less than 900 Cl; less than 900 Br; less than 1,500 total ppm IEC 61249-2-21; EN14582