GR900 | QFN Epoxy Molding Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

GR900C-Q1L4 | QFN Epoxy Molding Compound

Main features

  • Low stress and moisture absorption
  • High adhesion
  • Low moisture absorption

Product Description

Hysol GR900 is a green molding compound specifically developed for DFN/QFN MSL1 applications. It's designed to provide exceptional performance and reliability. The compound meets the UL94V-0 flammability standard at a thickness of 1/8 inch.

Product Key Features

  • Halogen-free
  • Low stress — Minimizes stress on delicate electronic components, enhancing long-term reliability.
  • High adhesion — Provides a strong bond to the substrate, preventing delamination.
  • Low moisture absorption — Reduces the risk of moisture-related defects.
  • High reliability — Ideal for demanding applications where durability and performance are critical.

Applications

  • DFN/QFNMSL1 Applications
Product Family

HYSOL GR900

1. Select Pellet Size
2. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Filler Content Filler Content
89 %
Filler Size Cut Filler Size Cut
53 µm
Specific Gravity Specific Gravity
2.00
Electrical Properties
Volume Resistivity Volume Resistivity
45e15 Ohms⋅cm
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
50 cm
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity Thermal Conductivity
0.9 W/m.K

Additional Information

Hysol GR900 Additional Handling Specification

Property Value Unit
Preheat Temperature 70 - 90 ℃
Molding Temperature 170 - 185 ℃
Molding Pressure 40 - 85 kg/cm²
Transfer Time (Conventional Mold) 8 - 15 s
Transfer Time (Automold) 8 - 15 s
Curing Time 110 - 150 s
Post Cure Time 4 - 8 h

 