Main features

  • For MnO Tantalum Capacitors
  • Black colored
  • Halogen-free version of MG33F-0602 & MG33F-0593

Product Description

Hysol GR2320 is a black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of Manganese Oxide or MnO2 tantalum capacitors. This laser markable product is filled by 71% filler weight, has low ionic impurities and excellent thermal cycling performance.

Hysol GR2320 is an Environmentally "Green" product that replaces MG33F-0602 & MG33F-0593. Environmentally "green", meaning that it doesn't contain any halogens including bromine, antimony or phosphorus flame retardants. MG33F-0602 & MG33F-0593 dominated the space for tantalum capacitors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products.

Hysol GR2320 is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on Maganese Oxide MnO2 capacitors. Its fast cure time also ensures that it is compatible with the latest automold manufacturing equipment while it also meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

 

Product Family

HYSOL GR2320

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Black
Filler Content Filler Content
71 %
Specific Gravity Specific Gravity
1.8
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
170 °C
Thermal Conductivity Thermal Conductivity
0.7 W/m.K
UL 94 Rating UL 94 Rating
V0
Electrical Properties
Volume Resistivity Volume Resistivity
10000000000000000 Ohms⋅cm
Mechanical Properties
Molded Shrinkage Molded Shrinkage
0.25 %
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
76.2 cm
Curing Conditions
Transfer Pressure Transfer Pressure
40 - 85 kg/cm2
Transfer Time Transfer Time
6 - 15 s