Hysol GR2310V | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR2310V Gold Long Flow Epoxy Mold Compound Hysol GR2310V | Gold Epoxy Mold Compound

Main features

  • Long flow version of GR2310
  • For MnO Tantalum Capacitors
  • Gold (yellow) colored

Product Description

Hysol GR2310V is a long flow, long-gel time version of GR2310. It is gold (yellow) in color and is a semiconductor-grade epoxy molding compound or duroplast designed for the encapsulation and protection of Manganese Oxide (MnO2) tantalum capacitors and automotive sensor packages. Once molded and post-mold cured, this product provides optimium protection and reliability for these capacitor devices.

Hysol GR2310V is a laser markable, environmentally "green" product, meaning that doesn't contain any halogens including bromine, antimony or phosphorus flame retardants. MG33F-0520 and MG33F-0602 dominated the space for tantalum capacitors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products. It is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature. Its fast cure time ensures that it is compatible with the latest automold manufacturing equipment. Hysol GR2310V meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

 

Product Family

HYSOL GR2310V

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Gold
Filler Content Filler Content
72 %
Specific Gravity Specific Gravity
1.85
Electrical Properties
Volume Resistivity Volume Resistivity
10000000000000000 Ohms⋅cm
Mechanical Properties
Molded Shrinkage Molded Shrinkage
0.3 %
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
180 °C
Thermal Conductivity Thermal Conductivity
0.7 W/m.K
UL 94 Rating UL 94 Rating
V0
Curing Conditions
Transfer Pressure Transfer Pressure
40 - 85 kg/cm2
Transfer Time Transfer Time
6 - 15 s
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
114 cm

Additional Information

Tantalum capacitors are general purpose mature products and as such, the products used to mold them must be cost-competitive. Although the GR2310V has "only" been manufactured for 15 years or so, it has been optimised as to offer the lowest cost possible for a non halogen containing formulation.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers