Hysol GR180T | White Epoxy Mold Compound

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

Hysol GR180T | White transmitting Epoxy Mold Compound Hysol GR180T | White Epoxy Mold Compound

Main features

  • Transmitting compound
  • High reliability
  • Good workability

Product Description

Hysol GR180T is a white, transmitting epoxy molding compound used for optical applications. This crystal silica filled (70%) product has been specifically designed to improve light transmittance and workability for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators.

Hysol GR180T cures with heat and has been developed to be workable for transfer molding processes. It has been formulated to provide the best possible moldability for a wide range of molding process parameters.

Product Family

HYSOL GR180T

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Filler Content Filler Content
70 %
Specific Gravity Specific Gravity
1.85
Chemical Properties
Moisture absorption Moisture absorption
0.67 %
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
73 cm
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
195 °C
Curing Conditions
Transfer Pressure Transfer Pressure
40 - 85 kg/cm2
Transfer Time Transfer Time
5 - 12 s

Additional Information

Storage

Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.

Leading Brands Trust in Our Products and Services