HumiSeal Thinner 602-245

Harmonization Code : 3814001000 |

HumiSeal Thinner 602-245

Main features

  • RoHS Directive 2011/65/EU compliant
  • For acrylic conformal coatings
  • Ensures proper viscosity adjustment

Product Description

HumiSeal Thinners are blends of solvents, formulated to maintain the original system balance when added to the correct coating type. These HumiSeal® Thinners are in full compliance with the RoHS Directive 2011/65/EU. 

Product Key Features

  • Ensures proper viscosity adjustment for HumiSeal conformal coatings
  • Fully compliant with RoHS Directive 2011/65/EU. 

Applications

  • Adjusting viscosity of HumiSeal acrylic-based conformal coatings
Product Family

HUMISEAL 602-245

1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Ketone
Color Color
Clear
Specific Gravity Specific Gravity
0.8
Vapor Density Vapor Density
3.45
Vapor Pressure Vapor Pressure
0.02148026 kg/cm2
Thermal Properties
Boiling Point Boiling Point
117 °C
Flash Point Flash Point
14 °C

Additional Information

Directions for Use   

Add HumiSeal® Thinner to a compatible coating until the desired viscosity is obtained.  

Handling Precautions  

HumiSeal® Thinners are flammable and the following standard safety precautions should be observed:  

  • Use only in well ventilated areas.   
  • Protective gloves and goggles should be worn.   
  • In case of prolonged skin contact, wash with water.   
  • In case of eye contact, flush with water and contact physician.   
  • Avoid prolonged breathing of vapors.  
  • Unused portions of HumiSeal® products must be disposed of in strict compliance with Local, State, and  Federal laws governing such matters.   
  • Consult the Safety Data Sheet (SDS) for more specific product information. 